1. Material of Core:Fe-base amorphous alloy ribbon
2. Dimensions of Core:


3. Magnetical Test:(AQL 0.65)
Test of Iron loss and AL according to GB/T 19346-2003( The test standard for Fe-base nanocrystalline alloy in China)
3.1 Loss Test:
Magnetic Induction Density:B=0.037T
Frequency:f=16kHz
Test Equipment:2010SA AC soft magnetic tester
Iron Loss:pFe≤1.2W/kg
AMCC-32 Iron Loss:PFe≤0.55W
3.2 AL Test:
We can be gained different permeability and inductance values by adjusting the air gap.