Waterproof cloth offset printing heat transfer sticker, using PET release film as substrate . Can be applied for waterproof cloth like raincoat, waterproof coat, waterproof apron etc.
Waterproof cloth offset printing heat transfer sticker, it is eco-friendly and with good washing and color fastness. can be washed 40-60times, 30mins/time. The waterproof cloth is needed to have the coating layer.
Heat Transfer Process:
· Use heat press machine .
· It is better to put the teflon cloth on the fabric when pressing.
Transfer Time
|
6-12s sec
|
Temperature
|
150-160℃
|
Transfer Pressure
|
20-30 Pound
|
Sheet Size
|
39*54cm & 48*64cm
|
Technology
|
Offset printing
|
Design Dimension
|
Customize Accepted
|
Massive production
|
4-7 working days, according to the quantity
|
Peeling Method
|
Cold & hot Peeling
|
Warranty
|
12 Months
|
Color
|
colorful
|
Application
|
Cotton,Textiles,Fabric,Blend, Clothing.Leather etc
|
Certificate
|
SGS
|
Service
|
Strongest Staff & Team,within 24 Hours Reply
|
OEM& Design
|
Available
|
Produce Process:
Waterproof cloth offset printing heat transfer sticker, it is produced by offset printing. It is produced by imported chemical materials.
Packing & shipping:
· For package, it is 100sheets in a bag and 500 sheets in a carton.
· For shipping, it can be shipped by air express ( TNT, DHL, FedEx etc) and by sea.
Our cooperative policy:
· Can be modified free of charge 1 times.
· to provide artwork design services.
· Quality problem 100% complement.
· The quality of the second shipment to produce freight Division I bear.
· Provide a pre-shipment that after hot test report and before hot test .
· Priority to get the our latest product information after our cooperation.
· Offering professional one-on-one service and replying your E-mail within three hours.
Commitment 100% Return Description:
· The color is wrong.
· Wash water fade, normal washing 10 times.
· The pattern size is inconsistent with the customer's sample.
· Tolerance is not allowed, leaked white (white print post moves).
· Adhesive is the whole expansion of 0.2mm, plastic edge is greater than 0.25mm or so, too large.
· The wrong pattern, and the drawings provided by the customer is inconsistent, the pattern is wrong.